DCIF Westerly Granite AE Stress Effect Test (Task 3-1)
Directional Cooling-Induced Fracturing (DCIF) experiments were conducted on rectangular Westerly granite blocks (width=depth=4.0", height=2.0"). Liquid nitrogen was poured in a... -
DCIF (Directional Cooling-Induced Fracturing) Westerly Granite AE Borehole Da...
Directional Cooling-Induced Fracturing (DCIF) experiments were conducted on three rectangular Westerly granite blocks (width=depth=4.0", height=2.0") which were preheated to...